Shrink marks occur on the surface of the injection molded part, which refers to the local depressions formed on the surface of the injection molded part. Sink marks are usually generated at the local thick wall of injection molded parts, or at the back of protrusions such as ribs and screw columns. On the injection molded parts of automobiles, the backside of structures such as screw posts, ribs or buckles are prone to sink marks.
Causes: Shrink marks are caused by the lack of effective pressure-retaining and shrinkage during the cooling of the injection molded parts.
solution:
For the sink marks on the back of the screw column, a common improvement measure is to add a crater structure at the root of the screw column. Reduce the equivalent wall thickness. The smaller the equivalent wall thickness, the less likely the sink marks will be on the surface of the injection molded part. When the equivalent wall thickness at the root of the screw column is close to the wall thickness T of the injection molded part, there is basically no risk of sink marks on the injection molded part.
Automobile injection parts generally use modified PP materials. Compared with engineering plastics, modified PP has a lower elastic modulus and a lower resistance to deformation. It is necessary to ensure the strength of injection molded parts from the structural design. A common method is to add ribs in product design. The choice of the thickness of the rib is related to whether shrinkage marks are produced on the surface of the injection molded part. For crystalline polymers, because the crystallization will cause post-shrinkage, the thickness of the rib root should be thinner. It is recommended not to exceed 1/3 of the wall thickness, otherwise it is easy to form shrink marks on the back; and for amorphous polymers, due to post-shrinkage Smaller, the thickness of the root of the rib can be appropriately thick, but it is recommended not to exceed 1/2 of the wall thickness. When the rib design is not reasonable, it is easy to form sink marks on the back. If possible, design the reinforcement ribs behind the transition surface where the two planes meet. Even if there are slight sink marks, the sink marks can be concealed ingeniously due to the masking effect of the protective surface.
Reasonable structural design. Car bumpers have strict requirements on appearance. Even if there are slight sink marks on the injection molded parts, they will be very obvious after painting, which puts higher requirements on the design of the structure. Due to the needs of assembly, automobile injection molded parts are often designed with many buckles behind the appearance. The size design of the buckle is very important. If the wall thickness is thin, the strength of the buckle is insufficient, and it is easy to produce a lack of glue during injection; thick wall thickness will produce sink marks. The best solution is to reduce the wall thickness of the buckle root, which not only solves the strength problem of the buckle, but also avoids sink marks, and at the same time ensures smooth injection molding. The buckle root is not thinned, and shrink marks are easily generated during injection molding.
Causes and methods of shrink marks on the surface of injection molded parts
Jun 10, 2020
Leave a message
Send Inquiry