The 7 factors to be considered when setting the injection molding process are as follows.


(1) Shrinkage rate
The form and calculation of thermoplastic molding shrinkage As mentioned above, the factors that affect thermoplastic molding shrinkage are as follows.
①Plastic varieties
During the thermoplastic molding process, due to the volume change in the form of crystallization, the internal stress is strong, and it freezes in the plastic part.
Compared with thermosetting plastics, the shrinkage rate is larger, the shrinkage rate range is wide,
The directionality is obvious, and the shrinkage after molding, annealing or humidity conditioning treatment is generally larger than that of thermosetting plastics.
②Characteristics of plastic parts
When the molten material is in contact with the surface of the cavity, the outer layer immediately cools to form a low-density solid shell. Due to the thermal conductivity of plastic
Poor performance, the plastic inner layer is slowly cooled to form a high-density solid layer with large shrinkage. So thick wall, slow cooling, high density layer
Thick ones shrink more. In addition, the presence or absence of inserts and the layout and quantity of inserts directly affect the flow direction, density distribution and shrinkage
The size of the resistance, etc., so the characteristics of the plastic parts have a great influence on the size and direction of the shrinkage.
③The form, size and distribution of the feeding port
These factors directly affect the material flow direction, distribution density, pressure-holding and feeding effect and molding time. direct feed inlet
If the section of the feed port is large (especially the thick section), the shrinkage will be small, but the directionality will be large. If the feed port width and length are short, the directionality will be small.
Close to the feed port or parallel to the direction of the material flow, the shrinkage is large.
④ Molding conditions
The mold temperature is high, the molten material cools slowly, the density is high, and the shrinkage is large, especially for the crystal material, the volume changes due to the high crystallinity.
The larger it is, the greater the shrinkage. The mold temperature distribution is also related to the cooling inside and outside the plastic parts and the density uniformity, which directly affects the quality of each part.
Shrink size and directionality. In addition, maintaining pressure and time also have a greater impact on contraction, and those with high pressure and long time will contract.
Small but directional. The injection pressure is high, the viscosity difference of the molten material is small, the interlayer shear stress is small, and the elastic rebound after demolding is large.
Therefore, the shrinkage can also be appropriately reduced, the material temperature is high, the shrinkage is large, but the directionality is small. Therefore, adjust the mold temperature, pressure,
Various factors such as injection speed and cooling time can also appropriately change the plastic shrinkage.
When designing the mold, according to the shrinkage range of various plastics, the wall thickness, shape, size and distribution of the feeding port,
Determine the shrinkage rate of each part of the plastic part according to experience, and then calculate the cavity size. For high-precision plastic parts and when it is difficult to grasp the shrinkage rate,
Generally, the following methods should be used to design the mold.
① Take the smaller shrinkage rate for the outer diameter of the plastic parts, and the larger shrinkage rate for the inner diameter, so as to leave room for correction after mold trial.
②The mold test determines the form, size and molding conditions of the gating system.
③The diameter of the plastic parts to be post-processed should be post-processed to determine the dimensional change (the measurement must be taken 24 hours after demoulding).
④ Correct the mold according to the actual shrinkage.
⑤ Retry the mold and change the process conditions appropriately, and slightly modify the shrinkage value to meet the requirements of the plastic parts.


(2) Liquidity
The fluidity of thermoplastics can generally be determined from molecular weight, melt index, Archimedes spiral flow length,
A series of indices such as apparent viscosity and flow ratio (process length/wall thickness of plastic parts) are analyzed. Small molecular weight, molecular weight fraction
Wide cloth, poor molecular structure regularity; high melt index, long spiral flow length, small apparent viscosity, and large flow ratio will flow
Sex is good. For the plastic of the same name, the instruction manual must be checked to determine whether its fluidity is suitable for injection molding. By mold
The design requirements can roughly divide the fluidity of commonly used plastics into three categories.
①Good fluidity PA, PE, PS, PP, CA, poly-4 methyl pentene.
②Polystyrene series values (such as ABS, AS), PMMA, POM, polyphenylene ether with medium fluidity.
③Poor fluidity PC, hard PVC, polyphenylene ether, polysulfone, polyarylsulfone, fluoroplastic.
The fluidity of various plastics also changes due to various molding factors. The main influencing factors are as follows:
①Temperature
When the material temperature is high, the fluidity increases, but different plastics are also different. PS (especially impact-resistant type and high MFR value),
The fluidity of PP, PA, PMMA, modified polystyrene (such as ABS, AS), PC, CA and other plastics varies greatly with temperature.
For PE and POM, the temperature increase or decrease has little effect on their fluidity. Therefore, the former should adjust the temperature to control the flow during molding
sex.
②Pressure
When the injection pressure increases, the molten material will be greatly sheared, and the fluidity will also increase, especially PE and POM are more sensitive, so
The fluidity should be controlled by adjusting the pressure of the injection molding machine during molding.
③Mold structure
Form, size, layout, cooling system design, molten material flow resistance (such as surface finish, material
Factors such as channel section thickness, cavity shape, exhaust system) directly affect the actual fluidity of the molten material in the cavity.
If the temperature of the molten material is reduced and the flow resistance is increased, the flowability will be reduced. Mold design should be based on the plastic used
the liquidity and choose a reasonable structure. During molding, the material temperature, mold temperature, injection pressure, injection speed and other factors can also be controlled.
To properly adjust the filling situation to meet the molding needs.


(3) Crystallinity
Thermoplastics can be divided into crystalline plastics and amorphous plastics (also known as amorphous plastics) according to whether they crystallize during condensation.
shape) two categories of plastics. The so-called crystallization phenomenon is that when the plastic changes from the molten state to the condensation, the molecules move freely (completely
in an out-of-order state) becomes stopped from free motion, in a slightly fixed position, and has a tendency to make the molecular arrangement a regular model
a phenomenon of direction.
As the appearance standard for judging these two types of plastics, it depends on the thickness of the plastic and the transparency of the plastic parts.
The material is opaque or translucent (such as POM, etc.), and the amorphous plastic is transparent (such as PMMA, etc.).
When designing a mold and selecting an injection molding machine, the following requirements and precautions for crystalline plastics should be noted.
①The heat required for the material temperature to rise to the molding temperature is large, and equipment with large plasticizing capacity should be used.
②When cooling, the heat is released, so it should be fully cooled.
③ The density difference between the molten state and the solid state is large, the molding shrinkage is large, and shrinkage holes and pores are prone to occur.
④Fast cooling, low crystallinity, small shrinkage and high transparency. The degree of crystallinity is related to the wall thickness of the plastic part, and the wall thickness is slow to cool and crystallize.
High strength, large shrinkage and good physical properties. Therefore, crystalline plastics should control the mold temperature as required.
⑤ Significant anisotropy and large internal stress. Uncrystallized molecules tend to continue to crystallize after demolding
Balanced state, prone to deformation and warping.
⑥ The crystallization temperature range is narrow, and it is easy to cause unmelted material not to be injected into the mold or to block the feeding port.


(4) Heat-sensitive plastics and easily hydrolyzed plastics
Thermal sensitivity means that some plastics are more sensitive to heat, and they are heated for a long time at high temperatures, or the cross section of the feed port is too small, and the shear
When the cutting action is large, the temperature of the material increases, and it is prone to discoloration, degradation and decomposition. Plastics with this characteristic are called heat-sensitive.
plastic. Such as rigid PVC, polyvinylidene chloride, vinyl acetate copolymer, POM, polychlorotrifluoroethylene, etc. heat sensitive plastics
Monomers, gases, solids and other by-products are generated during decomposition, especially some decomposition gases have thorns on the human body, equipment, and molds.
irritation, corrosive effect or toxicity. Therefore, attention should be paid to the selection of injection molding machines for mold design and molding, and screw injection molding should be selected.
The cross-section of the machine and gating system should be large, the mold and barrel should be chrome-plated, there should be no stagnation, and the molding temperature must be strictly controlled.
Stabilizers are added to plastics to weaken their heat-sensitive properties.
Some plastics (such as PC) will decompose under high temperature and high pressure even if they contain a small amount of moisture.
Easily hydrolyzed, it must be preheated and dried.


(5) Stress cracking and melt fracture
Some plastics are sensitive to stress, and are prone to internal stress during molding and are brittle and easy to crack.
Under the action, cracking occurs. For this reason, in addition to adding additives to the raw materials to improve the crack resistance, attention should be paid to the raw materials
Dry, reasonably select molding conditions to reduce internal stress and increase crack resistance. And should choose a reasonable shape of plastic parts, not
Measures such as inserts should be provided to minimize stress concentration. When designing the mold, the drafting slope should be increased, and a reasonable feeding port should be selected.
and ejection mechanism, the material temperature, mold temperature, injection pressure and cooling time should be properly adjusted during molding, and try to avoid plastic parts over
When it is cold and brittle, it is released from the mold. After molding, the plastic parts should be post-treated to improve crack resistance, eliminate internal stress and prohibit contact with solvents.
When the polymer melt with a certain flow rate passes through the nozzle hole at a constant temperature, the flow rate exceeds a certain value, and the melt surface occurs.
Obvious transverse cracks are called melt fractures, which damage the appearance and physical properties of plastic parts. Therefore, in the selection of polymers with high melt flow rate
When the nozzle, runner, and feed port cross-section should be increased, the injection speed should be reduced, and the material temperature should be increased.


(6) Thermal performance and cooling rate
Various plastics have different thermal properties such as specific heat capacity, thermal conductivity, and heat distortion temperature. Plasticizing with high specific heat capacity requires heat
If the quantity is large, the injection molding machine with large plasticizing capacity should be selected. The heat distortion temperature is high, the cooling time of the plastic is short, and the demoulding is early, but the demoulding
After cooling to prevent deformation. Plastics with low thermal conductivity have a slow cooling rate (such as ionic polymers, etc.), so they must
It must be fully cooled, and the cooling effect of the mold should be strengthened. Hot runner molds are suitable for plastics with low specific heat capacity and high thermal conductivity. specific heat
Plastics with large capacity, low thermal conductivity, low thermal deformation temperature and slow cooling rate are not conducive to high-speed molding, and appropriate plastics must be selected.
Injection molding machine and enhanced mold cooling.
Various plastics must maintain an appropriate cooling rate according to their type characteristics and plastic shape requirements. So the mold must be shaped according to the
A heating and cooling system is required to maintain a certain mold temperature. When the mold temperature rises, it should be cooled to prevent the plastic part from being demolded
After deformation, the molding cycle is shortened and the crystallinity is reduced. When the plastic waste heat is not enough to keep the mold at a certain temperature, the mold
A heating system should be provided to keep the mold at a certain temperature to control the cooling rate, ensure fluidity, and improve filling conditions.
Or used to control plastic parts to cool slowly, prevent uneven cooling inside and outside of thick-walled plastic parts and improve crystallinity. on liquidity
Good, large molding area, uneven material temperature, according to the molding situation of plastic parts, sometimes it is necessary to use alternately heating or cooling or local heating
Use with cooling. For this purpose, the mold should be equipped with a corresponding cooling or heating system.


(7) Hygroscopicity
There are various additives in plastics, which make them have different degrees of affinity for water, so plastics can be roughly divided into hygroscopic,
Adhesion to water and non-absorbing water are not easy to adhere to water. The water content in the material must be controlled within the allowable range.
Under high pressure, moisture becomes gas or hydrolysis occurs, which causes resin foaming, decreased fluidity, and poor appearance and mechanical properties.
Therefore, hygroscopic plastics must be preheated by appropriate heating methods and specifications as required to prevent re-hygroscopicity during use.