In the production process of aluminum alloy die castings, various defects often inevitably occur, one of the most complex and changeable defects is "strain".

The strain defect of aluminum alloy die-casting parts refers to the linear strain marks appearing in the mold opening direction when the aluminum alloy die-casting parts are separated from the mold. These marks usually have a certain depth. In severe cases, they may even cause the entire surface to appear. Strain conditions.

 

aluminum alloy die-casting

There are many reasons for strain defects in aluminum alloy die castings:

  1. Mold surface damage: Damage on the mold cavity surface, such as scratches or dents, will cause the molten metal to easily adhere when injected into the mold, causing strain defects.
  2. The mold ejection direction has no slope or the slope is too small: If the mold ejection direction does not have an appropriate slope or the slope is too small, it will increase the probability of adhesion between the molten metal and the mold surface, resulting in strain defects.
  3. Unbalanced ejection force: Uneven ejection force in different parts will cause the aluminum alloy die-casting parts to be subjected to uneven force during the de-molding process, which is prone to strain.
  4. Looseness of the mold: Looseness of the mold during the production process may cause gaps or irregular contacts between the inner surface of the mold and the aluminum liquid, resulting in strain defects. This cause is often difficult to detect.
  5. Pouring temperature is too high or too low: Although there are relatively few strain defects caused by this reason, a pouring temperature that is too high will cause the alloy liquid to adhere to the surface of the mold, increasing the probability of strain; while pouring temperature that is too low may As a result, the aluminum liquid solidifies too quickly, and strain defects can also occur.

 

To deal with the strain defects of aluminum alloy die castings, the following methods can be adopted:

  1. Repair the surface damage of the mold and ensure the smoothness of the mold cavity surface.
  2. Adjust the slope of the mold so that the slope in the mold ejection direction meets the requirements, reduce the adhesion of the molten metal to the mold surface, and reduce the occurrence of strain defects.
  3. Balance the ejection force to ensure uniform ejection force in different parts to avoid uneven force during the de-molding process, thereby reducing strain defects.
  4. Fasten the mold to ensure that the mold maintains a stable structure during the production process and avoid strain problems caused by loose mold.
  5. Control reasonable pouring temperature and mold temperature. According to the specific casting process requirements, control the pouring temperature and mold temperature within the appropriate range to avoid strain problems caused by too high or too low temperatures.
  6. Replace the release agent or use anti-strain paint. Choose a suitable release agent and ensure that it works well. Alternatively, consider using anti-strain paint to reduce the adhesion of the molten metal to the mold surface.
  7. Adjust the iron content of the aluminum alloy. Normally, the iron content should not be less than 0.8% to reduce the occurrence of strain defects.
  8. Adjust the cooling time and reasonably control the cooling time according to the specific casting process requirements to avoid strain problems caused by too long or too short cooling time.
  9. Modify the gate structure, change the flow direction of molten aluminum, reduce the adhesion of molten metal to the mold surface, and reduce the occurrence of strain defects.
  10. Ensure that the parallelism of the die-casting machine meets the requirements to avoid strain defects caused by uneven force.

To effectively solve the problem of strain defects in aluminum alloy die castings, it is necessary to comprehensively consider the above factors and adopt corresponding treatment methods.