Blogs

What are some of the injection molding defects

Mar 19, 2022 Leave a message


First, plastic is a wavy problem.

Cause.

Due to the gate or other parts of the narrow, molten plastic to promote the curing of plastic parts forward, the surface produces ripples.

Solution.

1. Increase the injection diameter

2. Improve the injection nozzle and mold temperature

3. Increase the height of the barrel

4. Speed up the injection speed

5. Slow down the injection speed

6. Change the cooling water inlet position of the mold so that it is far away from the gate.

7. Expand the gate.

Second, the plastic parts are silver patterned.

Cause.

Because the plastic contains moisture, uneven mixing, air entrapment during injection, too many additives or release agents.

Solution: 1.

1. Strengthen the back pressure

2. Slow down the injection speed

3. Clean up the barrel of the material

4. Increase the mold temperature

5. Change the location of the gate

6. Expand the runner and sprue

7. Bake the material

8. Install infrared light in the material door.


Three, the plastic interface is bad.

Cause.

Due to the plastic temperature is too low, can not melt, or due to gas drainage is not enough to cause more than two strands of shunt mixing and produce hair-like thin lines or bubbles.

Solution.

1. improve the material temperature

2. Increase the injection temperature

3. Increase the injection speed

4. Set up cold material pool outside the seam line

5. Set up air release port

6. Change the gate position or gate

7. Don't use release agent

8. Switch to low viscosity raw materials that are easy to flow.

Fourth, the plastic parts show hollow.

Cause.

Due to the plastic surface contact with the low-temperature mold wall during the melt curing, shrinkage is concentrated in the thick wall section and caused by the cavity, or due to the air entrapment made of the cavity.

Solution.

1. Increase the injection pressure (and secondary pressure)

2. extend the injection time

3. Reduce the barrel curing temperature

4. Reduce the wall thickness to below 6mm, if necessary, set the wall thickness to help line, and remove the excess wall thickness

5. Expand the gate

6. Shorten the flow channel

7. Adjust the mold temperature evenly

8. Change the location of the gate to exclude the air trap.

five. Plastic parts under-injection or lack of material.

Cause.

Due to insufficient mechanical injection and plasticizing performance, bad material flow, too thin gate cross-section, too thin mold wall or bad air release.

Solution.

1. Increase the injection rate, if still insufficient, it is necessary to change the heavy machinery

2. Install anti-leakage injection valve screw

3. Improve the injection pressure

4. Improve the barrel, injection nozzle curing and mold temperature

5. Check whether the electric hotline is disconnected

6. Check whether the injection nozzle is blocked, increase the cycle speed

7. Improve the air release capacity of the mold

8. Increase the cross-section of the gate

9. Increase product wall thickness

10. Add helper line, transform the material flow

11. Use low viscosity raw material

12. Add lubricant.


Sixth, the side of the mold extrusion plastic.

Cause.

Because the material temperature and injection pressure is too high, or clamping force is not enough.

Solution.

1. Reduce the injection pressure and barrel curing temperature

2. Shorten the injection time

3. Reduce the injection speed

4. Use high clamping force machine instead

5. Modify the clamping surface to fit tightly and clean the clamping surface

6. Switch to low viscosity material.

Seven, plastic surface dents.

Cause.

The surface of the plastic part is cooled at the wrong time, and the surface is dented.

Solution.

. Increase the rate of material injection

2. Increase the pressure in the mold groove (secondary pressure)

3. Reduce the curing temperature of the cylinder material

4. Increase the injection flow rate

5.Increase the injection rate

6. Extend the injection time

7. Make the mold temperature uniform

8. Change the gate position

9. Enlarge the gate

10. Shorten the mold runner.

Eight, the plastic part distortion deformation.

Cause.

Due to injection residual stress relaxation leads to distortion of plastic parts.

Solution.

1. Reduce the injection pressure

2. Reduce the barrel material curing temperature

3. Extend the cooling time

4. Adjust the wall thickness of the material and adjust the release lock action.

5. Add a mold release lock

6. Change the gate position

7. Adjust the mold temperature.

This injection molding knowledge is provided by MINDWELL injection molding engineers, MINDWELL is a professional injection molding production factory. We provide competitive and high-quality injection molded parts.

Send Inquiry